Long-term protective effect of surface sealants against erosive wear by intrinsic and extrinsic acids

Wegehaupt, Florian J ; Tauböck, Tobias T ; Sener, Beatrice ; Attin, Thomas

Journal of Dentistry, May 2012, Vol.40(5), pp.416-422 [Periódico revisado por pares]

Texto completo disponível

Citações Citado por
  • Título:
    Long-term protective effect of surface sealants against erosive wear by intrinsic and extrinsic acids
  • Autor: Wegehaupt, Florian J ; Tauböck, Tobias T ; Sener, Beatrice ; Attin, Thomas
  • Assuntos: Enamel ; Erosion ; Surface Sealant ; Hydrochloric Acid ; Citric Acid ; Enamel ; Erosion ; Surface Sealant ; Hydrochloric Acid ; Citric Acid ; Dentistry
  • É parte de: Journal of Dentistry, May 2012, Vol.40(5), pp.416-422
  • Descrição: To test sealants to prevent erosive tooth wear caused by extrinsic and intrinsic acids under long-term exposition. 144 bovine enamel samples were randomly allocated to twelve groups (1–12). Samples of groups 1, 5 and 9 remained unsealed (positive controls), 2, 6 and 10 were sealed with Silicon Seal Nano Mix and 3, 7 and 11 with Seal&Protect. Groups 4, 8 and 12 were sealed with flowable composite (negative controls). Groups 1–4 were immersed in artificial saliva, 5–8 in hydrochloric acid and groups 9–12 in citric acid for 28 days, respectively. After 1, 2, 4, 7, 11, 14, 21 and 28 days, solutions were renewed and enamel wear was quantified by assignation of 32P in the solutions. In all immersion solutions, lowest mineral loss was observed for the negative controls whilst highest loss was observed for unsealed positive controls. In artificial saliva and citric acid, the loss from samples sealed with Seal&Protect...